I have bought a large roll of wool/poly batting and as I have gotten through the roll I'm finding the inner stuff is very wrinkled/creased. I cut off what I need and give it a steam and light iron on a medium/low heat. I then leave it draped on the floor for a day or two to make sure there is no moisture left in it from the steaming. It reduces the creases substantially. This is a bothersome thing which I never really considered when buying my roll and despite the savings of buying in bulk, I just may not do it again because of this hassle.