Here is the setup i use. That is a plate of 3/8" steel that i use as a "heat sink"

[ATTACH=CONFIG]461210[/ATTACH]

Here we are stirring off the oxidized crud
[ATTACH=CONFIG]461211[/ATTACH]

Metal is poured...
[ATTACH=CONFIG]461212[/ATTACH]

The first cast! It usually takes a cast or two to heat the mold enough to let the metal flow completely. This one has a slight bubble at the arrow on the left.
[ATTACH=CONFIG]461213[/ATTACH]
Attached Thumbnails 2014-02-08-14.17.16.jpg   2014-02-08-14.37.08.jpg   2014-02-08-14.40.11.jpg   2014-02-08-14.42.47.jpg  